From: Olivier B. <olivier.2a@free.fr.invalid>
Newsgroups: fr.rec.bricolage
Subject: Re: =?ISO-8859-15?Q?B=E9ton_ou_mortier?=
Date: Thu, 22 Sep 2022 20:46:17 +0200
Organization: Aioe.org NNTP Server
Message-ID: <tgiahp$1ec1$1@gioia.aioe.org>
References: <632b00d9$0$2988$426a74cc@news.free.fr> <632b81da$0$22259$426a74cc@news.free.fr> <632ba165$0$22065$426a74cc@news.free.fr> <632c31e3$0$22078$426a74cc@news.free.fr> <632c39de$0$5119$426a74cc@news.free.fr>
Mime-Version: 1.0
Content-Type: text/plain; charset="iso-8859-15"; format=flowed
Content-Transfer-Encoding: 8bit
Injection-Info: gioia.aioe.org; logging-data="47489"; posting-host="2pe1QRMTcglVrgkTfV63pg.user.gioia.aioe.org"; mail-complaints-to="abuse@aioe.org";
X-Notice: Filtered by postfilter v. 0.9.2
X-Newsreader: MesNews/1.08.06.00-fr
Bytes: 1796
Lines: 18

Le 22/09/2022, Aegidius a supposé :

> J'avais déjà posté "Sur chantier on dit 3 brouettes 1 sac" si ça apparait en 
> double...
>
> Le sable de la plage n'est pas trop conseillé je ne sais pas pourquoi 
> peut-être le sel ?
>
je crois mais je pense aussi que le coté arrondi et souvent mono 
calibre des grains du sable de plage va à l'encontre d'une bonne 
imbrication lors du vibrage avec au final plus d'interstices et de 
ciment, et donc moins de solidité.

Dans une fabrique à béton j'ai dépanné une carte électronique de 
commande de production de ce qu'ils appellent "la fine", issu du 
rinçage des toupies ces petites particules sont rincées puis 
réintroduites dans le processus de fabrication du béton ce qui complète 
l'imbrication et leur permet de monter à une norme ISO-truc supérieure 
en terme de solidité.